| Property | Value |
|---|---|
| Filament Diameter | 1.75 mm ± 0.03 mm |
| Density | 1.80 g/cm³ |
| Glass Transition Temperature | 55–60 °C |
| Melting Point | 140–160 °C |
| Tensile Strength | ≥ 43 MPa |
| Elongation at Break | ≥ 4% |
| Impact Strength (Charpy, notched) | ≥ 3 kJ/m² |
| Printing Temperature | 190–230 °C |
| Bed Temperature | 0–60 °C |
| Spool Net Weight | Varies by product configuration |
| Property | Value |
|---|---|
| Filament Diameter | 1.75 mm ± 0.03 mm |
| Density | 1.80 g/cm³ |
| Glass Transition Temperature | 55–60 °C |
| Melting Point | 140–160 °C |
| Tensile Strength | ≥ 43 MPa |
| Elongation at Break | ≥ 4% |
| Impact Strength (Charpy, notched) | ≥ 3 kJ/m² |
| Printing Temperature | 190–230 °C |
| Bed Temperature | 0–60 °C |
| Spool Net Weight | Varies by product configuration |